Publication:
Synthesis and characterization of flexible zinc oxide-based composites

dc.contributor.advisor Perales-Pérez, Oscar J.
dc.contributor.author Duque-Saldarraiga, Santiago
dc.contributor.college College of Engineering en_US
dc.contributor.committee Quintero, Pedro
dc.contributor.committee Valentin, Ricky
dc.contributor.department Department of Mechanical Engineering en_US
dc.contributor.representative Lopez Moreno, Laura
dc.date.accessioned 2019-03-29T12:58:18Z
dc.date.available 2019-03-29T12:58:18Z
dc.date.issued 2018-12-12
dc.description.abstract An organic flexible optoelectronic device (f-OLED), composed by a conductive polymeric substrate (PEDOT:PSS) and a composition-controlled semiconductive layer of ZnO was designed based on the industry’s requirements of mechanical flexibility and cost-effective optical properties. ZnO-PEDOT:PSS was chosen due to its expected mechanical flexibility, low absorbance over 400nm to 700nm and tunable conductivity. Zinc oxide (ZnO) was selected as a potential replacement to ITO (Iridium Tin Oxide) due to its less fragile (brittle) behavior, which is a basic requirement on flexible composites. Based on the above considerations, nanocrystalline ZnO particles were dispersed at different loadings within the PEDOT:PSS matrix. The morphological, structural, mechanical and functional properties were determined for different w/w ratio of ZnO nanoparticles and overall film thickness. Two approaches were followed: A physical deposition of metallic Zn onto polymer surface and subsequent air oxidation, and a mechanical mixing of the ZnO nanocrystals with PEDOT:PSS matrix at the upper layers of the composite films. The morphological structure of the flexible optoelectronic composites was characterized via optical microscopy and scanning electron microscopy (SEM) allowing to assess the cluster structures of ZnO nanoparticles randomly dispersed in the composite. The composition was inspected via Fourier transformed infrared spectroscopy (FT-IR) and x-ray diffraction (XRD) allowing to determine mechanical adhesion as the prevailing mechanism since no component was altered during the fabrication process. Optical properties were inspected using an ultraviolet-visible spectrometer (UV-VIS) and a photoluminescent spectrometer (PL) detailing the characteristic exciton of pure ZnO at 372nm and its corresponding fluorescent emission at 388nm. Mechanical test where performed according to ASTM D682-1a results on a 15% ZnO - 85% PEDOT:PSS indicate over 1.3 GPa of Young Modulus a notable increase compared with 0.89 GPa of pristine PEDOT:PSS. It is possible to conclude that vacuum dried components outperformed those generated with a slight increase in thermal load. en_US
dc.description.graduationSemester Spring en_US
dc.description.graduationYear 2019 en_US
dc.identifier.uri https://hdl.handle.net/20.500.11801/1885
dc.language.iso en en_US
dc.rights.holder (c) 2018 Santiago Duque Saldarriaga en_US
dc.rights.license All rights reserved en_US
dc.subject ZnO en_US
dc.subject PEDOT:PSS en_US
dc.subject Composites en_US
dc.subject Flexible Optoelectronics en_US
dc.subject Thin Flim Composites en_US
dc.subject.lcsh Zinc oxide --Synthesis en_US
dc.subject.lcsh Composite materials en_US
dc.subject.lcsh Optoelectronics en_US
dc.subject.lcsh Polymers and polymerization -- Electric properties en_US
dc.subject.lcsh Fourier transform infrared spectroscopy en_US
dc.subject.lcsh Nanoparticles en_US
dc.title Synthesis and characterization of flexible zinc oxide-based composites en_US
dc.type Thesis en_US
dspace.entity.type Publication
thesis.degree.discipline Mechanical Engineering en_US
thesis.degree.level M.S. en_US
Files
Original bundle
Now showing 1 - 1 of 1
Thumbnail Image
Name:
INME_DuqueSaldarriagaS_2018.pdf
Size:
2.71 MB
Format:
Adobe Portable Document Format
Description:
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
1.64 KB
Format:
Item-specific license agreed upon to submission
Description: